MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Softell DKG 250N 722 Tan Thermoplastic Polyolefin, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Softell DKG 250N 722 Tan is a 25% glass filled, thermoplastic polyolefin elastomer compound for injection molding. It is typically used for automotive interior applications that require low gloss, soft touch, very high rigidity, impact and good scratch and mar resistance.

Status: Developmental

Availability: North America

Application: Interior Automotive Applications; Soft Touch Applications

Market: Automotive

Processing Method: Injection Molding

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183-1
Melt Flow 15.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPaISO 527-1, -2
Elongation at Yield 12.0 %ISO 527-1, -2
Flexural Modulus 2400 MPaISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
@Temperature -30.0 °C
ISO 180
 42.0 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 142 °CUnannealed; ISO 75B-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9801 / 324736

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.