MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo Magnum™ 358HP ABS, High Heat  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The Automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 130 to 590 J/m and heat distortion temperatures from 77.C to 90.C are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating.

MAGNUM 358 HP ABS resin is a high heat, low gloss resin having unannealed DTUL values of 90.C at 1.8 MPa loading. MAGNUM 358 HP ABS resin is often used in switch plates, demister grilles and door rollovers, and visor covers.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/in
Melt Flow 2.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 40.0 MPa5800 psiISO Data
Tensile Strength, Yield 47.6 MPa6900 psiASTM Data
Elongation at Break 15 %15 %ASTM Data
Tensile Modulus 2.34 GPa339 ksiASTM Data
Izod Impact, Notched 2.19 J/cm4.10 ft-lb/inASTM Data
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO Data, Low Temp
 NBNBISO Data
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO Data, Low Temp
 1.80 J/cm²8.57 ft-lb/in²ISO Data
Instrumented Impact Total Energy  21.0 J
@Temperature -30.0 °C
15.5 ft-lb
@Temperature -22.0 °F
 42.0 J
@Temperature 23.0 °C
31.0 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 77.4 µm/m-°C
@Temperature 20.0 °C
43.0 µin/in-°F
@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FUnannealed; ASTM Data
Vicat Softening Point 117 °C243 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Magnum™ 344HP ABS
Trinseo Magnum™ 344CC ABS
Trinseo Magnum™ 342EZ ABS, Medium Impact
Trinseo Magnum™ 357HP ABS, High Heat
Trinseo Magnum™ 780HP ABS, High Heat, High Impact

PZZDW089 / 34320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.