MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Bayoxide® E 8712 Technical Oxide
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No: 1317-61-9

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.60 g/cc0.166 lb/in³DIN EN ISO 787-10
Water Absorption <= 0.50 %<= 0.50 %DIN EN ISO 787-2
Particle Size 0.30 µm0.30 µm
pH 5.0 - 9.05.0 - 9.0DIN EN ISO 787-9
Specific Surface Area 7.0 - 10.5 m²/g7.0 - 10.5 m²/gISO 9277
 
Electrical PropertiesMetricEnglishComments
Magnetic Coercive Force, Hc 90 - 130 Oe90 - 130 OeCoercivity IHc
Magnetic Saturation Flux Density, Bmax 4910 - 5390 Gauss4910 - 5390 GaussSaturation magnetization Bs
Magnetic Remanence, Br 710 - 1130 Gauss710 - 1130 GaussRemanence Br
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Monthbulk bags
 60.0 Month60.0 Monthbags
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 >= 98 %>= 98 %
 
Descriptive Properties
Specifications12.3-19.6 emu/gRemanence Br
 84.9-93.3 emu/gSaturation magnetization Bs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8405 / 208798

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.