MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Osprey 317L Stainless Steel Powder (Grade 80% - 22)  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Particle size distribution 1-250 microns. Typical distribution:
  • 80% < 22 microns
  • 67% < 16 microns
  • 43% < 10 microns
  • 14% < 5 microns
Mean size is 12 microns.

SHAPE: Predominantly spherical. Chemical composition and particle size distribution can be adjusted to suit customers' requirements.

The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001.

Information provided to MatWeb by Osprey Metals, now Sandvik Osprey Ltd.

Key Words: Powder Metallurgy; UNS S31703, AISI 317L, ISO 683/13 24, ASME SA240, ASTM A167, ASTM A240, Metal Powder, Metal Injection Molding, MIM, Microfine
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 12 µm12 µmMean
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %Typical
 <= 0.030 %<= 0.030 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 62.53 %62.53 %As Balance
Manganese, Mn 1.4 %1.4 %Typical
 <= 2.0 %<= 2.0 %
Molybdenum, Mo 3.0 - 4.0 %3.0 - 4.0 %
Nickel, Ni 11 - 15 %11 - 15 %
Nitrogen, N 0.050 %0.050 %Typical
 <= 0.10 %<= 0.10 %
Silicon, Si 0.50 %0.50 %Typical
 <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
WC <= 0.045 %<= 0.045 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyramid Stainless Steel AISI 304/316L, STAINLESS STEEL SHEET NO.4 FINISH
Sandvik Osprey 317L Stainless Steel Powder (Grade 95% - 16)
AISI Type 317L Stainless Steel, annealed sheet
AISI Type 317L Stainless Steel, annealed tubing
AISI Type 317L Stainless Steel, annealed plate

NOSPR040 / 18562

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.