MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stable

Uses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection molding: Various

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47 - 53
@Time 5.00 sec
ASTM D2240
Tensile Strength 60.0 MPaASTM D412
Tensile Strength, Ultimate 46.8 MPa
@Treatment Temp. 70.0 °C,
Time 3.629e+6 sec
Water Immersion
 46.8 MPa
@Treatment Temp. 100 °C,
Time 2.42e+6 sec
Oven Aging
 48.0 MPa
@Treatment Temp. 70.0 °C,
Time 1.21e+6 sec
Water Immersion
 48.0 MPa
@Treatment Temp. 70.0 °C,
Time 2.42e+6 sec
Water Immersion
 49.2 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
Oven Aging
 60.0 MPa
@Treatment Temp. 70.0 °C,
Time 0.000 sec
Water Immersion
 60.0 MPa
@Treatment Temp. 100 °C,
Time 0.000 sec
Oven Aging
Elongation at Break 410 %ASTM D412
100% Modulus 0.0152 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0352 GPa
@Strain 300 %
ASTM D412
Tear Strength 190 pliTrousers; ASTM D470
Graves Tear Strength 810 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 81H18, 1000g; ASTM D3389 B
 
Thermal PropertiesOriginal ValueComments
Melting Point 150 °CDSC
Glass Transition Temp, Tg -33.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Zone 1 193 °CExtrusion
Zone 2 199 °CExtrusion
Zone 3 204 °CExtrusion
Zone 4 210 °CExtrusion
Adapter Temperature 210 °C5, Extrusion
Die Temperature 210 °C6, Zone 1, Extrusion
 210 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5707F1 Ester Based Thermoplastic Polyurethane

PNOVEON061 / 55329

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.