MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Bayhydrol® U XP 2750 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic, hydroxyfunctional polycarbonate ester-polyurethane dispersion, cosolvent-free. Binder for the formulation of water-reducible 2K-PUR coatings.

Properties / Applications: Bayhydrol U 2757 can be used in combination with flexible polyurethane dispersions, e.g. Bayhydrol UH 340/1, UH 650, UH 2305 and UH XP 2660 to formulate soft-touch coatings. In combination with polyacrylates, e.g. Bayhydrol A 2058 highly chemical resistant comfort coatings can be formulated. Suitable polyisocyanate components are e.g. Bayhydur® 302, 304, XP 2655 and also Desmodur® N 3600 and N 3900. Bayhydrol U 2757 is cosolvent-free. It can be used in the formulation of highly haptic soft-feel coatings. The product has high elasticity, good chemical resistance and good scratch resistance. As with any product, use of Bayhydrol U XP 2757 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccDIN EN ISO 2811
Volatiles 57 - 61 %57 - 61 %1g/1h/125°C; DIN EN ISO 3251
pH 7.0 - 9.07.0 - 9.010%; DIN ISO 976
Viscosity 100 - 1500 cP100 - 1500 cPD= approx. 40 s-1; DIN 53019
 
Chemical PropertiesMetricEnglishComments
Acid Value 25 - 2925 - 29[mg KOH/g]; DIN EN ISO 2114
 
Descriptive Properties
Content3.6%OH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0168 / 201951

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.