Product Description: Enflex V1045D BLK UV (thermoplastic vulcanizate) is a fully weatherable rigid black EDPM/PP compound. This weatherable grade is designed for injection molding, extrusion and blow molding applications, requiring moderate rigidity and high heat resistance. Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Processability; Good Weather Resistance; High Heat Resistance; Low Compression Set; Medium Rigidity; Oil Resistant; Ozone Resistant; Recyclable Material; Solvent Resistant; UV Resistant Appearance: Black Processing Method: Blow Molding; Extrusion; Injection Molding Information provided by Entec Polymers |