Westlake EF464 is a high melt index resin suggested for use in compounding applications, such as a carrier for concentrates.Application/Uses- Compounding
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |