MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals NILO® Alloy 475 Controlled-Expansion Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Iron Base

Material Notes: Inflection point 360°C. A nickel-iron-chromium controlled-expansion alloy containing 47% nickel. It is designed to have thermal-expansion characteristics that closely match those of the soft glasses of the lead or soda-lime type up to their annealing temperatures. The alloy is a particularly good match with L92 glass. Used for various glass-to-metal seals and for anode-cavity caps in television tubes. The standard product form is strip.

Data provided by the manufacturer, Special Metals.

Key Words: DIN 17745; Werkstoff Nr. 2.4486; AFNOR NF A54-301
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.18 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 520 MPa75400 psiAnnealed
Tensile Strength, Yield 180 MPa26100 psiAnnealed; 0.2% offset.
Elongation at Break 37 %37 %Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000850 ohm-cm0.0000850 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.20 µm/m-°C
@Temperature 20.0 - 100 °C
4.56 µin/in-°F
@Temperature 68.0 - 212 °F
 9.75 - 10.35 µm/m-°C
@Temperature 20.0 - 450 °C
5.42 - 5.750 µin/in-°F
@Temperature 68.0 - 842 °F
Thermal Conductivity 12.6 W/m-K87.4 BTU-in/hr-ft²-°F
Melting Point 1450 °C2640 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 4.8 %4.8 %
Iron, Fe 48 %48 %nominal; adjustable to meet expansion requirements
Nickel, Ni 47 %47 %nominal; adjustable to meet expansion requirements

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
ATI Allegheny Ludlum Sealmet® 485 Controlled Expansion Alloy
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
ATI Allegheny Ludlum 430 Ti Controlled Expansion Alloy, UNS K91800

NIND23 / 17527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.