Temper: Mill-hardened Temper, TM - Hard Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld Common Fabrication Processes: Forming and Bending; Stamping Typical uses: Connectors; Contacts; Switches and Relays; Terminals Applicable Specifications: Sheet & Strip – ASTM B422/B422M; Strip – ASTM B888/B88M |