MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SEKISUI SPI KYDEX® T MB Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® T MB is a proprietary thermoplastic sheet that is cost competitive with fire retardant ABS/PVC (FR-ABS) formulations but with significantly higher impact strength and extensibility. Antimicrobial protection is built-in to continuously fight the growth of microbes.

Since KYDEX® T MB is less hygroscopic, unlike FR-ABS, it typically does not require pre-drying, offers superior impact, more uniform forming with less wall thinning and offers significantly greater resistance to a broad range of corrosive chemicals and cleaning solutions. It is available in a wide range of aesthetic choices and is Underwriter’s Laboratories, Inc.® recognized Std 94 V-0, 5V.

Suggested Application:

  • Aircraft Interiors
  • Mass Transit Vehicle Interior Components
  • Equipment Housings
  • Medical Products
  • Kiosk Housings
Features:
  • Substitute for FR-ABS sheet with competitive pricing but superior cost/performance
  • Higher breakage resistance measured by the Notched Izod test than competitive thermoplastics
  • Available in thicknesses from 0.71mm (0.028”) and up, in eight textures, a variety of colors, custom blank sizes and low minimums
  • Among the most rigid of thermoforming materials with a modulus of elasticity of 2,482 MPa (360,000 psi)
  • Easy to form with excellent part definition and deep-draw characteristics
  • Recognized by Underwriter’s Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses
  • Form times similar to FR-ABS making it an easy transition from competitive products.
  • Antimicrobial protection inhibits the growth of bacteria that can cause stains, odors and product deterioration.
  • Antimicrobial protection is built-in to the sheet so it won’t wash or wear away and lasts for the lifetime of the product/sheet.
  • Antimicrobial protection keeps the surface cleaner between cleanings.

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Moisture Absorption 0.0800 %
@Time 86400 sec
0.0800 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 94.094.0ASTM D785
Tensile Strength 42.0 MPa6090 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Tensile Modulus 2.60 GPa377 ksiASTM D638
Flexural Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 2.48 GPa360 ksiASTM D790
Compressive Yield Strength 54.0 MPa7830 psiASTM D695
Compressive Modulus 3.30 GPa479 ksiASTM D695
Bearing Yield Strength <= 197 MPa<= 28600 psiASTM D953
 31.0 MPa
@Strain 4.00 %
4500 psi
@Strain 4.00 %
ASTM D953
Poissons Ratio 0.4330.433ASTM D638
Shear Strength 50.0 MPa7250 psiASTM D732
Izod Impact, Notched 8.01 J/cm15.0 ft-lb/inASTM D256
Gardner Impact >= 70.0 J>= 51.6 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 17.1 kV/mm434 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C168 °Fannealed; ASTM D648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Vertical BurnPass60 and 12 sec; FAR 25.853(a)(i) and FAR 25.853(a)(ii)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS510 / 325250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.