MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Cerama-Fab™ 665  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Potting/Casting Ceramic

Material Notes: Chemical setting. Two-part, ceramic that can be machined and sintered. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" depth, then air set for 2-4 hours and cured at 200 ºF prior to operation. Two-part systems are used to produce high temperature molds and fixtures.

Key Words: Ceramacast
Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Open Porosity 5.0 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 62.0 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+9 ohm-cm
Dielectric Strength 3.00 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.50 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 17.0 W/m-K
Maximum Service Temperature, Air 1150 °C
 
Descriptive Properties
ColorGray(unfired) pink (fired)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec GRADE A LAVA Machinable Ceramic
Wacker HDK® T40 Nutrition Silica
Pyrotek Pyrite N-17 Refractory Board
Dicor Castable Fluormica Glass-Ceramic
Aremco Ceramacast™ 646 Castable Ceramic

ZCAR037 / 518

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.