MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2014-T3
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Key Words: UNS A92014; AA2014-T3; Al2014-T3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  >= 405 MPa
@Thickness 0.508 - 0.991 mm
>= 58700 psi
@Thickness 0.0200 - 0.0390 in
Flat sheet
 >= 405 MPa
@Thickness 1.02 - 6.32 mm
>= 58700 psi
@Thickness 0.0400 - 0.249 in
Flat sheet
Tensile Strength, Yield  >= 240 MPa
@Thickness 0.508 - 0.991 mm
>= 34800 psi
@Thickness 0.0200 - 0.0390 in
Flat sheet
 >= 250 MPa
@Thickness 1.02 - 6.32 mm
>= 36300 psi
@Thickness 0.0400 - 0.249 in
Flat sheet
Elongation at Break  14 %
@Thickness 1.02 - 6.32 mm
14 %
@Thickness 0.0400 - 0.249 in
Flat sheet
 15 %
@Thickness 0.508 - 0.991 mm
15 %
@Thickness 0.0200 - 0.0390 in
Flat sheet
Modulus of Elasticity 72.4 GPa10500 ksi
Compressive Modulus 73.8 GPa10700 ksi
Poissons Ratio <= 0.33<= 0.33
Shear Modulus 28.0 GPa4060 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000510 ohm-cm0.00000510 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  20.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.6 µin/in-°F
@Temperature -58.0 - 68.0 °F
 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
12.5 µin/in-°F
@Temperature 68.0 - 212 °F
 23.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.0 µin/in-°F
@Temperature 68.0 - 392 °F
 24.4 µm/m-°C
@Temperature 20.0 - 300 °C
13.6 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 134 W/m-K930 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.45 - 95 %90.45 - 95 %
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 3.9 - 5.0 %3.9 - 5.0 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.20 - 0.80 %0.20 - 0.80 %
Manganese, Mn 0.40 - 1.2 %0.40 - 1.2 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 0.50 - 1.2 %0.50 - 1.2 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2014-T4; 2014-T451
Aluminum 2014-T6; 2014-T651
Aluminum 2014-O
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
Alclad Aluminum 2014-T3

MA2014T3 / 109163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.