MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

AGC LUMIFLON® LF-916F Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON fluoropolymer resins were developed in 1982 as the first solvent-soluble fluoropolymers in the world. LUMIFLON polymers consist of alternating fluoroethylene and alkyl vinyl ether segments (FEVE). The fluorinated segments provide outstanding UV stability, weather resistance, and chemical resistance, while the vinyl ether segments provide solvent compatibility and cross-linking sites. LUMIFLON resins are used to make ultra-weatherable coatings for architectural, aerospace, automotive, and industrial maintenance markets. LUMIFLON LF-916F is a low molecular weight, high OH number resin. When LF-916F is dissolved in the appropriate exempt solvents, zero and low VOC and HAPS-free fluorourethane coatings can be formulated. The resin is typically used in applications where outstanding weathering is required along with excellent chemical resistance. Markets include aerospace coatings, architectural coatings, heavy duty industrial coatings, automotive coatings, and coatings for concrete..

Product Characteristics:

  • High OH functionality
  • Excellent weatherability and water resistance, excellent chemical resistance
  • Good adhesion to primers, metals, fiberglass, plastics, and composites
  • Zero/low VOC and HAPS free coatings are possible
  • Wide range of gloss possible
  • Curable at both ambient and elevated temperatures
  • Suitable for shop and field applied coatings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/cc
Volatiles >= 1.0 %>= 1.0 %
 
Mechanical PropertiesMetricEnglishComments
Impact  >= 1.0
@Diameter 12.7 mm
>= 1.0
@Diameter 0.500 in
[m], Intrusion 0.5 kg; ASTM D2794
 >= 1.0
@Diameter 12.7 mm
>= 1.0
@Diameter 0.500 in
[m], Extrusion 0.5 kg; ASTM D2794
 
Thermal PropertiesMetricEnglishComments
Softening Point 117.5 °C243.5 °F
Glass Transition Temp, Tg 34.0 °C93.2 °F
 
Optical PropertiesMetricEnglishComments
Gloss 80 %80 %20°; ISO 2813
 90 %90 %60°; ISO 2813
 
Descriptive Properties
AppearancePale Yellow Flakes
HardnessFPencil, ASTM D3363
OH Number100[mg KOH/g]-polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fiberglass Grade B
S-Glass Fiber, Generic
Cancarb Thermax® Floform N990 Ultra-Pure Medium Thermal Carbon Black
Armstrong C-1/A Epoxy Adhesive
Armstrong A-701 Epoxy Adhesive

PAGCX138 / 191247

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.