MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

GLS Corporation Versaflex™ OM6050X-1 TPE Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Bonds to Nylon 6 & 6/6

General Versaflex® Information: Versaflex® TPE alloys create soft touch characteristics that can be customized to create the unique feel that various application require (tactile, slippery, wet grip, silky).

Information provided by GLS Corporation.

All information provided by GLS Corporation. GLS Corporation and PolyOne (now Avient) merged in 2008. This discontinued grade was produced by GLS Corporation and is in MatWeb with the GLS name for historical accuracy.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
Tensile Strength, Ultimate 3.65 MPa530 psi
Elongation at Break 490 %490 %
100% Modulus 2.34 MPa
@Strain 100 %
340 psi
@Strain 100 %
Tear Strength 24.5 kN/m140 pli
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHB
 
Descriptive Properties
ColorNatural

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZGLSCV16 / 42250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.