MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Atom Adhesives AA-BOND 201 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system contains no solvents, mixes easily at room temperature, and is suitable for high performance structural bonding applications where the combination of very fast room temperature curing coupled with low shrinkage and excellent mechanical and electrical properties is needed. AA-BOND 201 develops strong, tough bonds to metals, plastics, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. AA-BOND 201 is an excellent electrical insulator, and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds. AA-BOND 201 develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds.

Appearance: Hazy, light straw

Cure Type: Heat cure or Room Temperature

Benefits:

  • Resistant to many organic/inorganics
  • Strong bond strength
  • Great electrical insulator
  • Durable
Mix Ratio by weight: 100:93/Resin:Hardener

Substrates: Metals, ceramics, glass, glass fabrics, wood leather, rigid plastics, marble, stone, rock, concrete, sheetrock, plaster, cement and tile.

Typical Application: Anything requiring the unique properties this adhesive offers

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccmixed, uncured
Solids Content 100 %uncured
Viscosity 3600 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25
Adhesive Bond Strength 200 psi
Izod Impact, Notched 1.90 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+11 ohm-cm
Dielectric Constant 4.8
Dielectric Strength 410 kV/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 59.9 µm/m-°C
Maximum Service Temperature, Air 115 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 25.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 65.0 °C
 2.00 hour
@Temperature 25.0 °C
 30.0 min
@Temperature 65.0 °C
Pot Life 3.00 minuncured
Shelf Life 12.0 Monthuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saxonburg Ceramics S-405 Cordierite
3D Systems DuraForm® GF Glass Filled Nylon
GBC Grade 90 Alumina
GBC Grade 85 Alumina
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR

PATOM003 / 172318

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.