MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ascend Performance Materials Starflam® 366 BK13 PA66 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Starflam 366 BK13 (formerly Vydyne® ECO366 BK13) is a non-halogenated, unreinforced, flame-retardant PA66 compound designed with high comparative tracking index (CTI) and low corrosion for improved electrical contact performance. It has superior flow properties to assist in filling thin-walled, intricate parts with reduced warpage and reduced cycle time. It is lubricated for machine feed and easy mold release. It is f1 rated in black.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³DAM; ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.3 %2.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
@Thickness 2.00 mm
0.0090 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
0.012 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa8410 psi50% RH; ISO 527-2
 83.0 MPa12000 psiDAM; ISO 527-2
Elongation at Break 5.0 %5.0 %DAM; ISO 527-2
 6.0 %6.0 %50% RH; ISO 527-2
Flexural Strength 39.0 MPa5660 psi50% RH; ISO 178
 107 MPa15500 psiDAM; ISO 178
Flexural Modulus 1.35 GPa196 ksi50% RH; ISO 178
 3.90 GPa566 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 7.80 J/cm²
@Temperature -30.0 °C
37.1 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.340 J/cm²
@Temperature 23.0 °C
1.62 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.370 J/cm²
@Temperature -30.0 °C
1.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm
@Thickness 1.00 mm
1.00e+10 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Dielectric Strength 17.0 kV/mm
@Thickness 1.00 mm
432 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
120 - 180 sec
@Thickness 0.118 in
PLC 5; ASTM D 495
Comparative Tracking Index 600 V
@Thickness 3.00 mm
600 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 15 - 30 sec15 - 30 secPLC 3; UL 746
 30 - 60 sec30 - 60 secPLC 2; UL 746
High Amp Arc Ignition, HAI 30 - 60 arcs30 - 60 arcsPLC 2; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minUL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 265 °C509 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 240 °C464 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  120 °C
@Thickness 0.400 mm
248 °F
@Thickness 0.0157 in
UL 746
 120 °C
@Thickness 0.750 mm
248 °F
@Thickness 0.0295 in
UL 746
 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0591 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  75.0 °C
@Thickness 0.400 mm
167 °F
@Thickness 0.0157 in
UL 746
 80.0 °C
@Thickness 0.750 mm
176 °F
@Thickness 0.0295 in
UL 746
 80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
 80.0 °C
@Thickness 3.00 mm
176 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  105 °C
@Thickness 0.400 mm
221 °F
@Thickness 0.0157 in
UL 746
 110 °C
@Thickness 0.750 mm
230 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 35 %35 %DAM; EN ISO 4589-2
Glow Wire Ignition Temperature  700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-13
 960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-13
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Middle Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Front Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Nozzle Temperature 260 - 290 °C500 - 554 °FInjection
Melt Temperature 270 - 285 °C518 - 545 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Lubricant
AppearanceBlack
FeaturesCrack Resistant
 Ductile
 Flame Retardant
 Good Mold Release
 Good Toughness
 Halogen Content, None
 Low Density
 Lubricated
 Organic Heat Stabilized
FormsPellets
Outdoor Suitabilityf1UL 746C
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9105 / 287556

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.