MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPH 5042 Polypropylene, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Polypropylene PPH 5042 is homopolymer.

Application

ATOFINA Polypropylene PPH 5042 has been specially designed for extrusion-thermoforming, where it gives improved rigidity and impact resistance combined with high clarity, reduced cycle times and good antistatic properties.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ISO 2039-2
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-2
Elongation at Yield 9.0 %9.0 %ISO 527-2
Tensile Modulus 1.50 GPa218 ksiISO 527-2
Flexural Modulus 1.60 GPa232 ksiISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 179
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °F120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °F120°C per hour; ISO 75-2
Vicat Softening Point 95.0 °C203 °F50N-50°C per hour; ISO 306
 153 °C307 °F10N-50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Pro® 4006 TH Polypropylene
Braskem EP 440L Injection Molding Polypropylene
Braskem CP 405 XP Injection Molding Polypropylene
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer
Braskem CP 401 HC Injection Molding Polypropylene

PFINAA120 / 38556

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.