MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
NuSil MED-1511 Silicone, One part Adhesive - Unrestricted Medical Use
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and plastics. There are one-part and two-part adhesives, ranging in consistency from flowable to non-flowable (non-slump). Silicone primers are specially formulated silanes supplied in a solvent that are used to improve the bond strength between a silicone elastomer or adhesive and another substrate surface (silicone, metals, and certain plastics).

Important Properties of Adhesives: In general, silicone adhesives adhere well to substrates such as glass, aluminum, titanium, other silicones, and some ceramics. While various types of materials can be used as adhesives, silicones are consistently chosen for their many inherent properties and overall versatility. Advantages of these adhesives are as versatile as silicone itself:

  • Proven biocompatibility
  • Resistance to moisture
  • Ability to remain elastic at temperatures below 0 ºC
  • Ability to resist chemical breakdown at temperatures >200 ºC
  • Low modulus prevents warpage, delamination and substrate failure.
Comments: Flowable

Cure System: Acetoxy

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25Typical
 20 - 35Certified
Tensile Strength at Break 6.00 MPaCertified
 9.70 MPaTypical
Tensile Stress at Strain 110 psi
@Strain 200 %
Elongation at Break 450 %Certified
 750 %Typical
Tear Strength 52.0 pliCertified
 100 pliTypical
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 100 g/min
Cure Time 72.0 hour
@Temperature 25.0 °C
Working Life <= 10.0 min
@Temperature 25.0 °C
 
Descriptive Properties
Mix Ratio1-Part

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® H5520 High Density Polyethylene
Celanese Celcon® M25-01 High Molecular Weight Acetal Copolymer
AlphaGary PVC 2212/S-110 CLEAR 0003 Polyvinyl Chloride Thermoplastic
NuSil MED-4162 Specialty Dispersion - Restricted Medical Use
NuSil MED-1540 Silicone, One part Adhesive - Unrestricted Medical Use

PNUSIL269 / 141993

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.