MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NAECO® ELKON® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Molybdenum Alloy; Precious Metal; Silver Alloy; Refractory Metal

Material Notes: For arcing electrical contacts especially where low mass is required.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.22 g/cc0.3692 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8282
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000383 ohm-cm0.00000383 ohm-cm(45% IACS)
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 250 W/m-K1740 BTU-in/hr-ft²-°F
Melting Point 980 - 2610 °C1800 - 4730 °F
Solidus 980 °C1800 °F
Liquidus 2610 °C4730 °F
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 60 %60 %
Silver, Ag 40 %40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® ELKONIUM 46 Silver Alloy
NAECO® ELKON® G14 Tungsten Carbide Silver contact material ASTM 663, Class A, infiltrated
China Tungsten FeMo55-A Ferro Molybdenum
CMW® D158F Silver Graphite Contact Material
CMW® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

NCMV852 / 192426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.