MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.92 g/cc1.92 g/ccASTM 792
    Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
    Melt Flow 12 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    12 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 939310 seconds; ASTM D2240
    Hardness, Shore D 414110 seconds; ASTM D2240
    Tensile Strength, Yield 5.52 MPa800 psiElastic; ASTM D412
    Elongation at Break 320 %320 %Elastic; ASTM D412
    Flexural Modulus, 1% Secant 310 MPa45000 psiASTM D790
    Tear Strength 35.1 kN/m200 pliASTM D624
     
    Thermal PropertiesMetricEnglishComments
    Flame Spread 23 mm/min0.90 in/minFM VSS-302
     
    Processing PropertiesMetricEnglishComments
    Middle Barrel Temperature 210 °C410 °F
    Front Barrel Temperature 227 °C440 °F
    Nozzle Temperature 235 °C455 °F
    Mold Temperature 51.7 °C125 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
    Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer

    PMULTI064 / 53968

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.