MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silon TABOREN PC 29 T 30-001 Polypropylene, 30% Talc Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: TABOREN-PC 29 T 30-001 is a compound based on polypropylene block copolymer filled with 30% of talc, stabilized with an UV additive and high antioxidant content package. It is suitable for extrusion and blow molding applications in many industrial fields with stress put on excellent processability and good surface performance.

Information provided by Silon US LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183-1
Melt Flow 0.900 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.900 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.0 MPa3480 psiISO 527
Elongation at Break 30.0 %30.0 %ISO 527
Flexural Modulus 2.70 GPa392 ksiISO 178
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 148 °C298 °Fmethod A50; ISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 15.0 - 40.0 °C59.0 - 104 °FHopper
Zone 1 180 - 190 °C356 - 374 °F
Zone 2 190 - 200 °C374 - 392 °F
Zone 3 200 - 210 °C392 - 410 °F
Adapter Temperature 200 - 210 °C392 - 410 °F
Die Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 200 - 210 °C392 - 410 °F
Drying Temperature 80.0 °C
@Time 10800 sec
176 °F
@Time 3.00 hour
 
Descriptive Properties
AppearanceBlack
Screw LengthLength: 25D – 30D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSILOM9873 / 325199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.