MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, cleaning agents, water, seawater and other chemicals. Compared with other types of plastics, UBESTA is particularly resistant to oils, and it displays strong resistance to organic acids and metal chlorides which adversely affect Nylon 12 and Nylon 66

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.8 MPa97% Ret.
Tensile Strength, Yield 38.4 MPa92% Ret.
Elongation at Break 92.5 %116% Ret.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 °CFlange Temperature for T-Die Cast Film Extrusion
Zone 1 190 °CFor T-Die Cast Film Extrusion
 230 °CFor 8x1 mm Tube Extrusion
Zone 2 210 °CFor T-Die Cast Film Extrusion
 225 °CFor 8x1 mm Tube Extrusion
Zone 3 220 °CFor 8x1 mm Tube Extrusion
 230 °CFor T-Die Cast Film Extrusion
Zone 4 215 °CFor 8x1 mm Tube Extrusion
Die Temperature 446 °FFor T-Die Cast Film Extrusion
Die Opening 0.0400 cmFor T-Die Cast Film Extrusion
Roll Temperature 50.0 °CChill Roll Temperature for T-Die Cast Film Extrusion
Drying Temperature 80.0 °COption 1
 100 °COption 2
 110 °COption 3
Dry Time 2 - 4 hourOption 3
 4 - 6 hourOption 2
 6 - 8 hourOption 1
Screw Speed 15 - 76 rpmFor 8x1 mm Tube Extrusion
 
Descriptive Properties
C/R3-3.5:1For 8x1 mm Tube Extrusion
Calibrating Vacuum100 mbarFor 8x1 mm Tube Extrusion
Calibration 9.95 mmFor 8x1 mm Tube Extrusion
Compression Ratiomin 3:1For 8x1 mm Tube Extrusion
Die Diameter16 mmFor 8x1 mm Tube Extrusion
Die Width300 mmFor T-Die Cast Film Extrusion
Extruder Barmag, Screw Diameter = 30 mmFor T-Die Cast Film Extrusion
Extruder Characteristics65 mm screw diameterFor 8x1 mm Tube Extrusion
Film Thickness60 micronsFor T-Die Cast Film Extrusion
Haul Off Speed5 m/minFor T-Die Cast Film Extrusion
Haul Speed10-55 m/minFor 8x1 mm Tube Extrusion
L/D Ratio25:1For 8x1 mm Tube Extrusion
Length of Compression Zone30% of screw lengthFor 8x1 mm Tube Extrusion
Length of Feeding Zone30-40% of screw lengthFor 8x1 mm Tube Extrusion
Length of Metering Zone30-45% of screw lengthFor 8x1 mm Tube Extrusion
Mandrel Diameter12 mmFor 8x1 mm Tube Extrusion
Tensile Work To Break914 kJ/m2113% Ret.
Water Temperature10-18°CFor 8x1 mm Tube Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUBE126 / 71686

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.