MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CHT ALPA-LSR 120203 Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a 2-part addition cure silicone elastomer system for Liquid Injection Molding (LSR). After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at elevated temperatures, usually in the range of 100 °C to 180 °C. The cycle time depends mainly on the temperature and the shape of the mould. The cured rubber exhibits excellent physical and electrical properties.

Key Features

  • self adhesive to aluminum
  • low compression set
Application: ALPA-LSR 120203 is particularly suited for the production of gaskets & sealings. Self adhesive to metals without the use of primer. In order to achieve the described properties, the vulcanization time, if a hot-air oven is used, should be at least 45 minutes at 175 °C. If a heating press is used, at least 5 minutes at 175 °C are required. In addition a postcure 4 h at 200 °C is recommended.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccB; DIN 53 479
 1.10 g/ccA; DIN 53 479
Brookfield Viscosity 300000 cPB
 325000 cPMixed
 350000 cPA
Linear Mold Shrinkage <= 0.0010 cm/cm
Storage Temperature 0.000 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 23.5DIN 53 505
Tensile Strength 870 psiDIN 53 504, S 3 A
Elongation at Break 600 %DIN 53 504, S 3 A
Tear Strength 86.0 pliASTM D 624, Die B
Compression Set <= 25 %BS ISO 815-1
 
Processing PropertiesOriginal ValueComments
Cure Time >= 48.0 hourDe-mould Time / Full Cure
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancelight blue
Colorlight blueB
 light blueCured Product
 translucentA
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL159 / 314642

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.