MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

REXtac Rextac® RT 1230 Amorphous Polyalphaolefin (APAO)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyalphaolefin; Polyolefin

Material Notes:
Laminate Grade.

Description: Ethylene copolymer and FDA compliant

Features: Good heat resistance, short open time, and excellent wetting properties

Applications: Lamination of reinforced tapes and protective overwraps

Other Properties:
Ring and Ball Softening Point (ASTM E 28): 143°C.
Needle Penetration (ASTM D 1321): 13 mm.
Shear Adhesion Failure Temperature (SAFT), Kraft/Kraft (Huntsman Method): 112°C.
Open Time, Kraft/Kraft (Huntsman Method): 10 sec.
Melt Density (190°C; Huntsman Method): 0.74 g/cc.
Flashpoint, COC (ASTM D 93): >235°C.

Information provided by Huntsman Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³ASTM D 792
Melt Density  0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
 0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
Viscosity 3000 cP
@Temperature 190 °C
3000 cP
@Temperature 374 °F
melt viscosity; ASTM D 3236
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1.03 MPa149 psiASTM D 638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 112 °C234 °FShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
 112 °C234 °FShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
Glass Transition Temp, Tg -22.0 °C-7.60 °FASTM D3417
Flash Point >= 235 °C>= 455 °FCOC; ASTM D 93
 >= 235 °C>= 455 °FCOC; ASTM D 93
Ring & Ball Softening Point 143 °C289 °FASTM E 28
 143 °C289 °FASTM E 28
 
Processing PropertiesMetricEnglishComments
Pot Life 0.167 min0.167 minOpen Time, Kraft/Kraft; Huntsman Method
 0.167 min0.167 minOpen Time, Kraft/Kraft; Huntsman Method
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 YesYes
 
Descriptive Properties
Needle Penetration (mm)13ASTM D 1321

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUN16 / 47636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.