MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChenGuang HGA-50 Two Component Silicone Rubber for Baby Nipple
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Molecule Formula: [Si(CH3)3O]n[Si(CH3)(CH=CH2)O]m

Properties:

  • Colorless, odorless, non-toxic, non-impurity material.
  • Mixing with reinforcer, structure controller and curing agent etc, it could be made into various kinds of articles by normal processing methods.
  • Excellent insulation property.
  • Good electric arc resistance, corona resistance and electric spark resistance.
  • Good water-proof, moisture-proof, unti-impact and unti-vibration properties.
  • Good physiological inertia and good air permeation property.
Applications: It suitable to be used in the fields of aviation, navigation, instrument and meter, electronic equipment, metallurgical, mechanics, automobile industries and medical purpose etc. It can be made into sealing rings, gaskets, tubes, cables, as well as human being organs, baby nipples, blood vessel, air permeable films, rubber mould and release agent of the precision mould casting.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 48 - 56JIS K6301
Tensile Strength at Break >= 7.00 MPaJIS K6301
Elongation at Break >= 400 %JIS K6301
Tear Strength >= 30.0 kN/mJIS K6301 (B)
Tensile Set <= 10 %JIS K6301
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU060 / 255659

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.