MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Moisture Absorption at Equilibrium 2.2 %in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 6.5 %in water at 23°C; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 240 MPavalue at 30 sec.; ISO 2039-1
Tensile Strength, Yield 230 MPav = 50 mm/min; ISO 527-2
Elongation at Break 2.5 %ISO 527-2
Tensile Modulus 17.0 GPaISO 527-2
Flexural Modulus 14.0 GPaISO 178
Charpy Impact Unnotched 6.00 J/cm²ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359
Thermal Conductivity 0.430 W/m-K
Melting Point 260 °C10K/min; ISO 3146
Maximum Service Temperature, Air 180 °CLong Term
 240 °CShort term
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-2
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Overview of materials for Nylon 6, Carbon Fiber Filled
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry)

PCENTR12 / 27963

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.