MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik TROGAMID® eCO myCX BC40 I Microcrystalline, permanently transparent polyamide, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: TROGAMID® eCO myCX BC40 I is a microcrystalline transparent polyamide for the manufacture of parts in the optical industry, like lenses, by injection molding. eCO stands for Evoniks aim to eliminate CO2 through use of renewable or circular feedstocks via massbalance approach. TROGAMID® eCO myCX BC40 I is supplied as spherical pellets in moisture-proof packaging. Preliminary data sheet.
Industrial Sector: Sustainable, Optics, Sports and Lifestyle
Sustainability: eCO
Processing: Injection molding , Extrusion
Optics: Transparent, High gloss, X-ray transparent
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Fatigue resistance
Conformity: Food contact
Additives: Unfilled
Applications: Fiber optic cable, (Sun-) glasses, Hygiene and cosmetics, Lenses, Monofilament
Processing: Film extrusion
Special Characteristics: Halogen-free, Phosphorus-free, High impact strength, Low viscosity
Features: optical UV-protection, Weldable, Low birefringence, Non-corrosive, Dishwasher detergents resistant
Regulatory: Food contact 10/2011/EC
Color: Blue
Delivery form: Spherical pellets

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiISO 527
Tensile Strength 63.0 MPa9140 psiISO 527
Tensile Stress 39.0 MPa
@Strain 50.0 %
5660 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 63.0 MPa9140 psiISO 527
Elongation at Break 185 %185 %Nominal; ISO 527
Elongation at Yield 7.00 %7.00 %ISO 527
Tensile Modulus 1.49 GPa216 ksiISO 527
Flexural Strength 54.0 MPa7830 psiat conv. Deflection; ISO 178
 88.0 MPa12800 psiISO 178
Flexural Modulus 1.50 GPa218 ksiISO 178
Flexural Strain at Break 8.00 %8.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 1.20 J/cm²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
Type of failure: C; ISO 179/1eA
 
Descriptive Properties
Blue water consumption12.4 kgISO 14040, 14044
ColorBlue
Global Warming Potential4.1 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 5.1 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.5 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7827 / 324959

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.