MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 893-10 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release, CALIBRE 893: Mold release and UV stabilizer.

Main Characteristics:

  • Underwriters Laboratory (UL)
Applications:
  • Electronics
  • Business equipment
  • Appliances

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4; ASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 59ASTM D785
Hardness, Rockwell R 123ASTM D785
Tensile Strength at Break 58.6 MPa50 mm/min; ASTM D638
 59.0 MPaISO 527-2/50
Tensile Strength, Yield 61.0 MPaISO 527-2/50
 61.4 MPa50 mm/min; ASTM D638
Elongation at Break 120 %50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2380 MPa50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 97.9 MPaMethod I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Flexural Modulus 2330 MPaMethod I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Izod Impact, Notched 690 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 68.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Tensile Impact Strength 630 kJ/m²ASTM D1822
Dart Drop, Total Energy 62.1 J3.39 m/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 137 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CUnannealed; ASTM D648
Vicat Softening Point 151 °C
@Load 5.10 kg
Rate A (50°C/h); ASTM D1525
Flammability, UL94 V-0
@Thickness 1.59 mm
 V-0
@Thickness 3.20 mm
 5VB
@Thickness 3.20 mm
Oxygen Index 36 %ASTM 2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 893-10 Polycarbonate

PZZDWST031 / 142240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.