MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reliance Industries Repol T100MK Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol T100MK is recommended for use in injection molding & stretch blow molding processes. It is an ideal material for attaining high clarity in housewares, syringes and ISBM products. Repol T100MK contains clarifier and antistatic agent that reduces static charge buildup on products.

Features:

  • Consistent processability
  • Good clarity
  • Good impact strength
  • Superior mechanical properties
  • Low static charge build-up and reduced dust pickup
  • Information provided by Reliance Industries

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Melt Flow 10 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    10 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Yield 28.0 MPa4060 psi50mm/min; ASTM D638
    Elongation at Yield 12 %12 %50mm/min; ASTM D638
    Flexural Modulus, 1% Secant 1000 MPa145000 psiASTM D790A
    Izod Impact, Notched 0.750 J/cm
    @Temperature 23.0 °C
    1.41 ft-lb/in
    @Temperature 73.4 °F
    ASTM D256
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 145 °C293 °FDSC second heating; ASTM D3418
    Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Reliance Industries Repol R019MZ Polypropylene
    Reliance Industries Repol R110MK Polypropylene
    Reliance Industries Repol H080EY Polypropylene
    Reliance Industries Repol H007EG Polypropylene
    Reliance Industries Repol C015EG Polypropylene

    PREL051 / 65391

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.