MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fibre Glast 83 Waxed Polyester Laminating Resin
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Description: #83 Waxed Polyester Laminating Resin is a prepromoted, thixotropic general purpose resin. #83 contains styrene wax for low styrene emissions and to prevent air inhibition. #83 is a waxed resin for laminating thin fiberglass skins on plywood, or for general purpose fiberglass repairs. The wax in the resin will prevent surface tackiness even when applied in thin coats. Sand off the wax layer before painting or secondary bonding.

Performance:
  • High thixotropic index to prevent draining in vertical surfaces
  • Low viscosity for fast wet out
  • Styrene suppressed

Suggested Uses:#83 Polyester Molding Resin can be used for hand lay-up or spray-up for general fiberglass reinforced plastics applications.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 56 %56 %
Brookfield Viscosity 475 cP475 cP#2 Spindle, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 22.8 - 37.8 °C73.0 - 100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 25.0 °C
0.500 hour
@Temperature 77.0 °F
using 1.25% #69 Catalyst
Gel Time 15.0 min15.0 minAt 77°F using 1.25% #69 Catalyst
 
Descriptive Properties
Maximum Exotherm320°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFIBRE28 / 38295

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.