MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Dover Chemical DOVERPHOS 49 Tris (Tridecyl) Phosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos 49 chemically is Tris (Tridecyl) Phosphite (TTDP). It is the highest molecular weight and lowest phosphorus content alkyl phosphate commercially available from Dover. Doverphos 49 has low volatility and good hydrolytic stability. Doverphos 49 is an effective stabilizer in conjunction with mixed metal heat stabilizers used in PVC. Typical use levels range from 0.25 to 1.00%

Information provided by DoverChem

Key Words: CAS# 68610-62-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.882 - 0.900 g/cc25°C/15.5°C
Molecular Weight 628 g/mol
ASTM Color <= 50APHA
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.10[mgKOH/gm]
 
Optical PropertiesOriginal ValueComments
Refractive Index <= 1.465
@Temperature 25.0 °C
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 4.9 %
 
Descriptive Properties
Physical FormClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER042 / 217661

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.