MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 58.4 microns2.30 milAdhesive
 107 microns4.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.75598 kN/m4.3125 pliPolypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 0.7669 kN/m4.375 pliABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 0.77789 kN/m4.4375 pliStainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 0.8108 kN/m4.625 pliPolypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 0.82172 kN/m4.6875 pliStainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 0.86554 kN/m4.9375 pliABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 
Descriptive Properties
Liner58# Polycoated kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M 9462P Adhesive Transfer Tapes with Adhesive 100

PMM33223 / 167970

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.