MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Llumar Sunrise Bronze V33BR SR CDF Window Film
Categories: Polymer; Film

Material Notes: Dual-Reflective films offer superior energy savings through lower interior reflectivity and higher exterior reflectivity allowing for excellent views to the outside both day and night. Dual-Reflective films are suggested for residential and commercial applications where heat and glare are the primary concerns.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 39 %
UV Transmittance 25 %Solar
Reflection Coefficient, Visible (0-1) 0.18Visible Reflectance (interior)
 0.25Visible Reflectance (exterior)
 0.43Total Solar Reflectance
 
Descriptive Properties
% Glare Reduction57
% Summer Solar Heat Gain Reduction60
% Total Solar Energy Rejected66
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction9
Emissivity0.67
Light to solar gain (LSG)1.15
Shading coefficient0.39
Solar absorption32
Solar Heat Gain Coefficient0.34
U-value0.95Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5454 / 222648

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.