MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Llumar Harmony Terre V31 SR CDF Window Film
Categories: Polymer; Film

Material Notes: Harmony films utilize proprietary metals and ceramic layers designed to provide superior heat rejection and moderate glare control with extremely low interior and exterior reflectivity.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 35 %35 %
UV Transmittance 19 %19 %Solar
Reflection Coefficient, Visible (0-1) 0.0600.060Visible Reflectance (exterior)
 0.0800.080Visible Reflectance (interior)
 0.220.22Total Solar Reflectance
 
Descriptive Properties
% Glare Reduction61
% Summer Solar Heat Gain Reduction59
% Total Solar Energy Rejected65
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction14
Emissivity0.57
Light to solar gain (LSG)1
Shading coefficient0.4
Solar absorption49
Solar Heat Gain Coefficient0.35
U-value0.89Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5445 / 222639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.