MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kohesi Bond KB 1613 RLV One component, low viscosity epoxy for underfill and potting applications
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Thermally conductive
  • Castable up to 1 inch thicknesses
  • Rapid cures at elevated temperatures
  • Superior dimensional stability
  • Exceptional electrical isolator
  • Unlimited working life at room temperature
Kohesi Bond KB 1613 RLV is a true single component system that requires no mixing and cures hard at elevated temperatures. Although it requires a minimum temperature of 120°C for curing (at which it cures extraordinarily fast), it can achieve even faster cures at elevated temperatures. KB 1613 RLV offers an extensive service temperature range of -50°C to +180°C. This product’s flow properties makes it ideal for use in underfill, potting and encapsulation applications. Being a one component system, it provides ease of application and also adheres well to an variety of substrates including metals, ceramics, most plastics and glass. It provides sterling mechanical strength properties and dimensional stability. KB 1613 RLV offers phenomenal thermal conductivity of 1 - 1.2 W/m/K. In addition to superior electrical insulation, KB 1613 RLV also offers chemical resistance to a variety of fuels, oils and water. It has a light yellow color, but it can be color matched to your specifications upon request. With a combination of Excellent performance, ease of use and excellent mechanical strength properties, KB 1613 RLV is widely used in electronics and microelectronics packaging and assembly applications.

Typical Applications:

  • Underfill
  • Coating
  • Sealing
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 10000 - 40000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 75
Tensile Strength >= 7200 psi
Compressive Strength >= 14500 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.53
@Frequency 60 Hz
Dielectric Strength >= 430 V/mil
@Thickness 3.17 mm
Dissipation Factor 0.033
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.00 - 1.20 W/m-K
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 15.0 min
@Temperature 150 °C
Option 2
 25.0 - 30.0 min
@Temperature 120 °C
Option 1
Shelf Life 6.00 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOHESI958 / 249137

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.