Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene products. It complies with US FDA 21CFR177.1520. Slip and antiblock addition distinguishes 142F from 142B. Applications: General purpose, trash bags, and liners. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |