MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Kalrez® 1058 FFKM Perfluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1050LF. Typically used in applications that require low sealing force or high extensibility including liquid chromatography septa, seals/seats for relief valves and tubing. Its shrinkage is higher than other Kalrez compounds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 - 2.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60 - 70ASTM D2240
Tensile Strength, Ultimate 9.00 MPaASTM D412
Elongation at Break 180 %ASTM D412
100% Modulus 0.00470 GPa
@Strain 100 %
ASTM D412
Tear Strength 3.06 kN/m
Compression Set 40 %
@Temperature 204 °C
70 hr at 204°C; ASTM D395B; Pellets
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.00e+17 ohm-cm
Dielectric Constant 4.9
@Frequency 1000 Hz
Dielectric Strength >= 17.7 kV/mm
Dissipation Factor 0.0050
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 229 µm/m-°C
@Temperature 22.0 - 100 °C
 230 µm/m-°C
@Temperature 22.0 - 260 °C
Specific Heat Capacity 0.945 J/g-°C
@Temperature 50.0 °C
 0.974 J/g-°C
@Temperature 100 °C
 1.053 J/g-°C
@Temperature 150 °C
Thermal Conductivity 0.170 W/m-K
@Temperature 200 °C
 0.180 W/m-K
@Temperature 100 °C
 0.190 W/m-K
@Temperature 50.0 °C
Maximum Service Temperature, Air 260 °C
Brittleness Temperature -40.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 7075 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8475 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 1050LF FFKM Perfluoroelastomer

PDVD02 / 33866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.