MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate (PC)

Material Notes: Foam thickness 0.250 in. Properties values at foam density of 0.90 g/cc.

Information provided by Bayer Corporation, Plastics Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Key Words: PC+ABS; Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccFoam; ASTM D792
 1.18 g/ccSolid; ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 42.0 MPaASTM D638
Elongation at Break 3.4 %ASTM D638
Flexural Yield Strength 80.0 MPaat 5% strain; ASTM D790
Flexural Modulus 2.62 GPaASTM D790
Impact Test 30.0 J
@Thickness 3.20 mm
Instrumented Impact, Total Energy; 3.2 mm thick, 2.5 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 6.35 mm
ASTM D648
UL RTI, Electrical 60.0 °C
@Thickness 3.00 mm
UL RTI, Mechanical with Impact 60.0 °C
@Thickness 3.00 mm
UL RTI, Mechanical without Impact 60.0 °C
@Thickness 3.00 mm
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 3.00 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Dow AIM® 4800 High Impact Styrenic Resin
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Bamberger Polymers Bapolene® 3262 Polyethylene, Injection Grade
Chevron Phillips EB6400 HIPS - High Impact Polystyrene

PB1B10 / 26403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.