MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin ER006987 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ ER006987 resin is a 30% glass reinforced blend of impact modified polyphenylene ether (PPE) + polystyrene (PS). This injection moldable material is FC EU, FDA food contact compliant, NSF/ANSI 61, ACS, WRAS, KTW, and W270 listing for global potable water use for specific colors is pending. NORYL ER006987 resin exhibits good fatigue performance, excellent long-term hydrolytic stability, very low moisture absorption, heat / hot water resistance and is an excellent candidate for a variety of water management applications such as pump housings, impellers, shower/faucet, membrane housings and valves.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 26 cP
@Load 10.0 kg,
Temperature 300 °C
26 cP
@Load 22.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Melt Flow 30 g/10 min
@Load 10.0 kg,
Temperature 300 °C
30 g/10 min
@Load 22.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 131 MPa19000 psi5 mm/min; ASTM D638
 131 MPa19000 psi5 mm/min; ISO 527
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527
 3.0 %3.0 %5 mm/min; ASTM D638
Tensile Modulus 9.425 GPa1367 ksi5 mm/min; ASTM D638
 9.475 GPa1374 ksi1 mm/min; ISO 527
Flexural Strength 188 MPa27300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 200 MPa29000 psibreak, 2mm/min; ISO 178
Flexural Modulus 7.65 GPa1110 ksi1.3 mm/min, 50 mm span; ASTM D790
 8.44 GPa1220 ksi2 mm/min; ISO 178
Izod Impact Notched 105 J77.4 ft-lbASTM D256
 85.0 J
@Temperature -30.0 °C
62.7 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.20 J/cm9.74 ft-lb/inASTM D4812
 5.50 J/cm
@Temperature -30.0 °C
10.3 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²20.0 ft-lb/in²80*10*4; ISO 180/1U
 45.0 kJ/m²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 153 °C
@Thickness 3.20 mm
307 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 147 °C
@Thickness 3.20 mm
297 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 154 °C309 °FRate B/50; ISO 306
 156 °C313 °FRate B/120; ISO 306
 164 °C327 °FRate A/50; ISO 306
 167 °C333 °FRate A/120; ISO 306
Glow Wire Ignition Temperature  800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
Glow Wire Flammability Index  775 °C
@Thickness 3.00 mm
1430 °F
@Thickness 0.118 in
IEC 60695-2-12
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 320 °C554 - 608 °F
Zone 2 280 - 300 °C536 - 572 °F
Zone 3 300 - 310 °C572 - 590 °F
Melt Temperature 290 - 320 °C554 - 608 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82282 / 290229

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.