MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraiburg TPE THERMOLAST® H RF9OGMLCNT Thermoplastic Elastomer (RC/FC/PCR/AP Series) Adhesion to PP
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The RC/FC/PCR/AP series is a material solution with post-consumer recycled content (hardness-dependent) for a variety of applications with adhesion to PP or for single component parts in Asia Pacific. The compounds are available in natural colors and precoloration is possible.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Translucent
  • Natural
Typical applications:
  • Function and design elements
  • Grip applications
  • Handles and grips for consumer applications
  • Toothbrushes
  • Razors
  • Toys
  • Household articles
  • Seals for housings
Material advantages:
  • Adhesion to PP
  • Alternative material to EPDM and PVC-P
  • Optimized mechanical properties
  • Non-sticky surface
  • Colorable
  • Temperature stability up to 80 °C
  • Soft, non-sticky haptic
  • Precoloration in all colors
  • Sustainable material

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN ISO 48-4
Tensile Strength 20.0 MPa2900 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 630 %630 %200 mm/min; DIN 53504/ISO 37
Tear Strength 35.0 kN/m200 pliISO 34-1 Method B (b)
 
Descriptive Properties
ColorNatural
Recycled raw materials content (%)38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8461 / 309125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.