MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik MHOROMER® BM 601 Dimethylaminoethyl Methacrylate  (discontinued **)
Categories: Fluid

Material Notes: Application: Water soluble polymers. Flocculants.

Appearance: Clear, colorless to yellowish liquid.

Odor: Amine-like

CAS: 2867-47-2

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³
Viscosity 1.6 cP
@Temperature 20.0 °C
1.6 cP
@Temperature 68.0 °F
Molecular Weight 157.2 g/mol157.2 g/mol
Vapor Pressure 0.0133 bar
@Temperature 75.0 °C
9.98 torr
@Temperature 167 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point 182 °C
@Pressure 0.1013 MPa
360 °F
@Pressure 14.69 psi
Flash Point 74.0 °C165 °FDIN 51758
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44
@Temperature 20.0 °C
1.44
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.050 %<= 0.050 %Rohm Method: M3 (according to K. Fischer)
 
Descriptive Properties
Colormax. 50Rohm Method: M5 (Pt-Co)
Degree of Purity (%)min. 99Rohm Method: M2-13 (GC)
Heat of Vaporization (kJ/mol)49.4
MEHQ720-880ppm, Rohm Method: M1-1 (HPLC), MEHQ
Solidification Point (°C)-30
Solubility (%)soluble in water

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik ROHAMERE® 6954-O Methacrylic Ester Of An Ethoxylated C16-C18 Fatty Alcohol Spectrum
Evonik MHOROMER® Ultra High Purity HEMA 2-Hydroxyethyl Methacrylate
Evonik MHOROMER® BM 923 2-Hydroxyethyl Methacrylate
Evonik MHOROMER® BM 903 2-Hydroxyethyl Methacrylate
Evonik MHOROMER® BM 711 Cyclohexyl Methacrylate

PCYR00083 / 101072

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.