MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Hytrel® PC956 NC010 TPC-ET  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 55 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Density 1.03 g/cc
@Temperature >=201 °C
Water Absorption 0.60 %
@Time 86400 sec
Sim. to ISO 62
 0.60 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
Melt Flow 6.8 g/10 min
@Load 2.16 kg,
Temperature 220 °C
from MVR and melt density; ISO 1133
 7.8 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ISO 7619-1
 51
@Time 15.0 sec
ISO 7619-1
Tensile Strength at Break 40.0 MPaISO 527-1/-2
Tensile Stress at Strain 6.90 MPa
@Strain 5.0 %
ISO 527-1/-2
 11.0 MPa
@Strain 10 %
ISO 527-1/-2
 14.5 MPa
@Strain 50 %
ISO 527-1/-2
 16.0 MPa
@Strain 100 %
ISO 527-1/-2
Elongation at Break >= 300 %ISO 527-1/-2
 600 %ISO 527-1/-2
Tensile Modulus 180 MPaISO 527-1/-2
Flexural Modulus 190 MPaISO 178
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180/1A
 NB
@Temperature -40.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 145 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 145 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Impact 300
@Temperature 23.0 °C
Tensile notched impact strength; ISO 8256/1
Tensile Creep Modulus, 1 hour 170 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 133 MPaISO 899-1
Tear Strength 134 kN/mnormal; ISO 34-1
 137 kN/mparallel; ISO 34-1
Abrasion 120mm3; ISO 4649
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.4
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 19.0 kV/mmIEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 180 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 177 µm/m-°CISO 11359-1/-2
Melting Point 201 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Vicat Softening Point 75.0 °C50°C/h, 50N; ISO 306
 180 °C50°C/h, 10N; ISO 306
Brittleness Temperature -98.0 °CISO 974
Glass Transition Temp, Tg -20.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
Oxygen Index 20 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 °CExtrusion Optimum
 220 - 235 °CExtrusion
 230 °CInjection Optimum
 220 - 250 °CInjection
Mold Temperature 45.0 °CInjection Optimum
 45.0 - 55.0 °CInjection
Drying Temperature 90.0 °CExtrusion
 100 °CInjection
 110 °CExtrusion
Dry Time 2.00 - 3.00 hourDehumidified Dryer; Extrusion
 2.00 - 3.00 hourDehumidified Dryer; Injection
Moisture Content 0.060 %Extrusion
 0.080 %Injection
 
Descriptive Properties
Delivery formPellets
Drying RecommendedyesInjection
Part Marking CodeTPC-ETISO 11469
ProcessingCasting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Resin IdentificationTPC-ETISO 1043
Special characteristicsLight stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8341C BK320 TPC-ET
Celanese Hytrel® HTR8223 BK320 TPC-ET
DuPont Mobility and Materials Hytrel® HTR8341G BK320 TPC-ET
BASF Elastollan® 1185 A M TPUR
Celanese Hytrel® HTR8206 TPC-ET

PDSX5225 / 197865

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.