MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Axiall 19920 Wire & Cable Flexible PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Non-lead stabilized 105°C insulation compound recommended for THHN-THWN circuit sizes. Well suited for 105°C; 1/64 wall in all AWG sizes. CSA approved for FT1 TWN75, TEW and AWM IA constructions. UL recognized for THHN, THWN, THW and TW.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 - 1.35 g/cc1.31 - 1.35 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 89 - 9589 - 95delayed; ASTM D-2240
Tensile Strength, Yield 19.7 MPa2850 psiASTM D-638
Elongation at Yield 288.1 %288.1 %Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
 330 %330 %ASTM D-638
100% Modulus 13.8 MPa
@Strain 100 %
2000 psi
@Strain 100 %
ASTM D-638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm50% RH; ASTM D-257
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -25.0 °C-13.0 °FASTM D-746
Oxygen Index 29 %29 %ASTM D-638
 
Processing PropertiesMetricEnglishComments
Melt Temperature 188 °C370 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® High Flow FMX1-9494 FEP Foam Concentrates
AlphaGary Garaflex™ E 4771-A8 OR1 LCF Vinyl Thermoplastic Elastomer
AlphaGary Garaflex™ E 4362 A1 LCF Vinyl Thermoplastic Elastomer
Axiall 22851 Coax & Telecom Flexible PVC
Geon® Performance Solutions Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible

PGGUL332 / 41608

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.