MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 8650H Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Post oil quenched hardness 61 HRC surface, 61 HRC half-radius, 61 HRC center.

Applications: torsion bar springs.

Key Words: UNS H86500, ASTM A304, SAE J1268
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 241
@Diameter 102 mm
 277
@Diameter 50.8 mm
 285
@Diameter 25.4 mm
 293
@Diameter 12.7 mm
Hardness, Knoop 265
@Diameter 102 mm
Converted from Brinell
 302
@Diameter 50.8 mm
Converted from Brinell
 311
@Diameter 25.4 mm
Converted from Brinell
 319
@Diameter 12.7 mm
Converted from Brinell
Hardness, Rockwell B 97
@Diameter 102 mm
Converted from Brinell
 99
@Diameter 12.7 mm
Converted from Brinell
 99
@Diameter 25.4 mm
Converted from Brinell
 99
@Diameter 50.8 mm
Converted from Brinell
Hardness, Rockwell C 22
@Diameter 102 mm
Converted from Brinell
 28
@Diameter 50.8 mm
Converted from Brinell
 30
@Diameter 25.4 mm
Converted from Brinell
 31
@Diameter 12.7 mm
Converted from Brinell
Hardness, Vickers 254
@Diameter 102 mm
Converted from Brinell
 292
@Diameter 50.8 mm
Converted from Brinell
 301
@Diameter 25.4 mm
Converted from Brinell
 309
@Diameter 12.7 mm
Converted from Brinell
Tensile Strength, Ultimate 841 MPa
@Diameter 102 mm
 931 MPa
@Diameter 50.8 mm
 972 MPa
@Diameter 25.4 mm
 1020 MPa
@Diameter 12.7 mm
Tensile Strength, Yield 650 MPa
@Diameter 102 mm
 834 MPa
@Diameter 50.8 mm
 910 MPa
@Diameter 25.4 mm
 945 MPa
@Diameter 12.7 mm
Elongation at Break 18.5 %
@Diameter 12.7 mm
in 50 mm
 19.5 %
@Diameter 25.4 mm
in 50 mm
 21.2 %
@Diameter 50.8 mm
in 50 mm
 22.5 %
@Diameter 102 mm
in 50 mm
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Calculated
Machinability 60 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000234 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical steel
Thermal Conductivity 46.6 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.47 - 0.54 %
Chromium, Cr 0.35 - 0.65 %
Iron, Fe 96.33 - 97.83 %As remainder
Manganese, Mn 0.70 - 1.05 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.35 - 0.75 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.045 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8650H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, round
AISI 8650H Steel, annealed, 25 mm (1 in.) round
AISI 8650H Steel, normalized 870°C (1600°F)
AISI 8650H Steel, normalized, 13 mm (0.5 in.) round
AISI 8650H Steel, normalized, 25 mm (1 in.) round

M865BN / 8541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.