MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21TDC-2LOND Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Electrically insulating
  • Paste consistency
  • Thermally conductive
  • Low outgassing system
  • Cryogenically serviceable down to 4K
  • High peel strength and elongation
Product Description: Master Bond EP21TDC-2LOND is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulated to cure fully at room temperature or more quickly at elevated temperatures with the optimum being overnight at room temperature followed by 2-3 hours at 200°F. It has an easy to use one to three mixing ratio by weight. It has a smooth paste like consistency with a non-drip application feature. EP21TDC-2LOND has outstanding toughness and combines flexibility and low outgassing. The cured compound exhibits a high elongation (greater than 25%), truly exceptional for a thermally conductive epoxy. EP21TDC-2LOND produces very little heat after mixing, which allows for a long working life. This epoxy resin compound exhibits good tensile shear and peel strength for bonding and sealing many different substrates including metals, glass, ceramics, rubber and many plastics. The cured epoxy is an excellent electrical insulator with superior chemical resistance to water, oils and fuels. Most noteworthy is its ability to withstand thermal shock, thermal cycling and mechanical shock. It has a service temperature range of 4K to +250°F and has been successfully employed in a number of cryogenic applications. Master Bond EP21TDC-2LOND is an exceptionally versatile system that offers the structural benefits of an epoxy, yet incorporates flexibility and very good thermal conductivity. It is widely used in the electronic, electro-optical and related industries. The color of Part A is gray; Part B is off-white.

Product Advantages:

  • Convenient mixing: non-critical one to three mix ratio by weight
  • Smooth paste consistency spreads evenly; long working life
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures
  • High peel strength and elongation
  • Cryogenically serviceable down to 4K
  • Superior bonding properties on similar and dissimilar substrates, superb impact resistance
  • Excellent flexibility; exceptional thermal shock and resistance to rigorous thermal cycling
  • High thermal conductivity combined with good electrical insulation properties
  • Low outgassing

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30 - 40
Tensile Strength >= 3000 psi
Elongation at Break >= 25 %
Adhesive Bond Strength >= 800 psiTensile lap, Aluminum to Aluminum
Peel Strength >= 15.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 90.0 µm/m-°C
Thermal Conductivity 1.2981 - 1.4423 W/m-K
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -269 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 48.0 - 72.0 hour
@Temperature 23.9 °C
Working Life >= 60.0 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Cure ScheduleOvernight at 75°Ffollowed by 2-3 hours at 150-200°F, Optimum cure
Mixing Ratio1:3 by weightParts A to B
ViscositypastePart A
 pastePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP36AO One Part, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Master Bond EP38FLAO Two Component Epoxy
Master Bond EP90FR-HFL Two Component Epoxy

PMASTM834 / 185427

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.