MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Dow™ DGDB-2480 NT HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow HDPE DGDB-2480 NT resin is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Suitable applications include natural gas distribution pipes, large diameter industrial piping, mining, sewage, and municipal water service lines.
Industrial Standards Compliance: ASTM D3350: cell classification
  • Natural – PE3455464A
  • Black – PE345464C (See NOTES A)
Plastics Pipe Institute (PPI): TR-4
  • Natural Pipe – DGDB-2480 NT 3408: ASTM PE3608 Pipe grade – 1600 psi HDB @ 73°F
  • Black Pipe – DGDB-2480 BK 3408 (See NOTES B): ASTM PE3608 Pipe grade – 1600 psi HDB @ 73°F and 800psi HDB @ 140°F
National Sanitation Foundation (NSF)
Standard 14 and 61
  • Natural Pipe – DGDB-24800 NT 3608
  • Black Pipe – DGDB-2480 BK 3608 (see NOTES B)
Consult the regulations for complete details.

Notes: (A) The first five numbers of the cell classification are based on natural resin. The last number and letter are based on black resin (natural resin plus 6.5% DFNF-0092).(B) Natural resin extruded under proper conditions with carbon black masterbatch DFNF-009 (6.5%)

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: ASTM D3350 PE345464A; ASMT D3350 PE345464C; NSF STD-14; NSF STD-61; PPI TR-4

Form: Pellets

Processing Method: Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccNatural resin; ASTM D792
 0.956 g/ccNatural resin extruded under proper conditions with carbon black masterbatch DFNF-0092 (6.5%); ASTM D792
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 8.3 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT 200 hour
@Temperature 80.0 °C
Slow Crack Growth; ASTM F1473
Tensile Strength, Yield 3200 psiASTM D638
Elongation at Break 850 %ASTM D638
Flexural Modulus 120000 psi2.4 MPa, Method I (3 point load); ASTM D790B
Izod Impact, Notched 4.00 ft-lb/inASTM D256A
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -148 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 440 °F
 
Descriptive Properties
Thermal Stability>482°FASTM D3350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF438 / 311131

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.