MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Pyro-Log Standard R-Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro Log is the only 152mm thick, high purity, needled blanket available in standard uncompressed densities up to 240kg/m3. Vertically-fiberized Pyro-Log fiber is of exceptional uniformity of dimensions and of naturally low shot content. Pyro-Log offers a unique solution to the problems encountered in designing linings for use in the toughest of furnace environments.

Applications: Pyro Log has a multitude of uses in heat containment applications in all industry groups, a selection of which are as follows:

  • Ceramic Industry (kiln car insulation - furnace floors)
  • Iron and Steel (walking beam furnace skid rail insulation)
  • General (engineered shapes)
  • Pyro-Log is the precursor material for the Pyro-Bloc range of mechanically fixed modules

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³uncompressed
 0.192 g/cc0.00694 lb/in³uncompressed
 0.240 g/cc0.00867 lb/in³uncompressed
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1080 °C
0.270 BTU/lb-°F
@Temperature 1980 °F
Thermal Conductivity  0.0700 W/m-K
@Temperature 400 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 240 kg/m3, blanket laid; ASTM
 0.0800 W/m-K
@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 192 kg/m3, blanket laid; ASTM
 0.0800 W/m-K
@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 160 kg/m3, blanket laid; ASTM
 0.100 W/m-K
@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 240 kg/m3, blanket laid; ASTM
 0.110 W/m-K
@Temperature 600 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 192 kg/m3, blanket laid; ASTM
 0.120 W/m-K
@Temperature 600 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 160 kg/m3, blanket laid; ASTM
 0.130 W/m-K
@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 240 kg/m3, blanket laid; ASTM
 0.150 W/m-K
@Temperature 800 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 192 kg/m3, blanket laid; ASTM
 0.170 W/m-K
@Temperature 1000 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 240 kg/m3, blanket laid; ASTM
 0.170 W/m-K
@Temperature 800 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 160 kg/m3, blanket laid; ASTM
 0.190 W/m-K
@Temperature 1000 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 192 kg/m3, blanket laid; ASTM
 0.220 W/m-K
@Temperature 1000 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 160 kg/m3, blanket laid; ASTM
Maximum Service Temperature, Air 1260 °C2300 °F
Shrinkage  1.6 %
@Temperature 1000 °C,
Time 86400 sec
1.6 %
@Temperature 1830 °F,
Time 24.0 hour
permanent, isothermal
 2.3 %
@Temperature 1100 °C,
Time 86400 sec
2.3 %
@Temperature 2010 °F,
Time 24.0 hour
permanent, isothermal
 3.0 %
@Temperature 1200 °C,
Time 86400 sec
3.0 %
@Temperature 2190 °F,
Time 24.0 hour
permanent, isothermal
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 0.25 %
@Temperature 800 °C,
Time 7200 sec
<= 0.25 %
@Temperature 1470 °F,
Time 2.00 hour
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF7023 / 203322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.