ALLEN® 2093MG is a general purpose ABS that has high impact strength and a good cost to performance ratio to other materials like stainless steel and other thermoplastics. ALLEN® 2093MG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302). Suggested Application: - Covers for food processing equipment
- Splash zone guards
- Deli risers
Features: - Custom color matching
- Medium gloss finish
Information provided by SEKISUI KYDEX, LLC. |