MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang F2311Q Fluoroelastomer Copolymer Gum
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Description: copolymer of VdF and CTFE

Molecular Formula : -[(CH2CF2)-(CF2CFCl)]n-

Properties: With good corrosion-resistance, strong-oxidant-resistance, and acid-resistance in special, such as fuming nitric acid, concentrated hydrochloric acid, hydrogen peroxide, etc. Good heat-resistance, good physical and mechanical and insulation properties. Working under 200 °C for long period. Working at 250°C for short period. Brittle point is at between -20~-40 °C

. Main Applications: Widely used in aviation, automobile, petroleum, and chemical industries, etc. Can be made into rubber belt, tube, film, fiberboned sheet and gasket, fuel tank and as dipping material.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1.5 - 2.4 cP1.5 - 2.4 cPIntrinsic, (30°C,acetone),100ml/g, Gum (before vulcanization)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 14.7 MPa>= 2130 psiVulcanized Elastomer
Elongation at Break >= 200 %>= 200 %Vulcanized Elastomer
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.10e+14 ohm-cm1.10e+14 ohm-cmGum (before vulcanization)
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 19.1 - 20.2 %19.1 - 20.2 %Gum (before vulcanization)
 
Descriptive Properties
Acid Resistance>6%weight increase at (18°C ~28°C) X 168hr in 96% nitric acid), Gum (before vulcanization)
Voltage at Break Down>21 MV/mGum (before vulcanization)
Weight Loss<0.3%at 200°CX24hr, Gum (before vulcanization)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU000 / 255599

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.